Brief Introduction to Physical & Chemical Performance Indicators, Magnesia-Carbon Brick Price

2026-05-21 16:10:38
times
Indicators include chemical composition, refractoriness, refractoriness under load, permanent linear change on reheating, apparent porosity, bulk density, mechanical strength (cold crushing strength & cold modulus of rupture), thermal shock resistance, thermal expansion coefficient, thermal conductivity, deformation resistance, etc.

1. Refractoriness

It refers to the capacity of refractories to resist melting under high temperatures. Under specified test conditions, heat magnesia-carbon bricks for converters, magnesia-carbon bricks for electric arc furnaces, special-shaped magnesia-carbon bricks and fired magnesia-chrome bricks. The equivalent temperature at which partial melting and certain softening occur is taken as the index. Refractoriness is mainly determined by chemical and mineral composition.

2. Refractoriness Under Load (RUL)

Also named load deformation temperature or load softening point. It stands for the resistance of refractory samples to combined high temperature and constant compressive load. The heating-up method is widely adopted domestically: under a static load of 0.2 MPa, heat samples at a standardized heating rate and record the temperatures corresponding to different deformation degrees.

3. Permanent Linear Change on Reheating

It describes irreversible length change of fired refractory products after reheating to high temperature, expressed as the percentage of length variation before and after heating. Positive values indicate expansion while negative values represent shrinkage. This index partially reflects high-temperature volume stability; for products with identical chemical composition, it serves as a marker of sintering degree.

4. Apparent Porosity

The ratio of open pore volume to the total volume of the refractory material. Apparent porosity generally reflects the compactness of refractories.

5. Bulk Density

The ratio of the material’s mass to its total volume, which characterizes the densification level of the product.

6. Thermal Shock Resistance

Also called thermal cycling resistance. It is the ability to withstand drastic temperature fluctuations (rapid heating & rapid cooling) without cracking or breaking. The water quenching method is commonly used in China: samples are cycled between 1100 °C and cold water for testing.

Functional Introduction of Continuous Casting Refractory Components

Stirring by purging plugs exerts a vital effect on homogenizing molten steel composition and temperature, and accelerates alloying.
Long nozzles and submerged entry nozzles (SEN) shield molten steel from secondary oxidation. Meanwhile, SEN regulate flow field inside the mold, which greatly facilitates inclusion floatation, reduces slag entrapment and stabilizes molten steel flow.
Silicon-free and carbon-free anti-clogging submerged entry nozzles not only prevent carbon and silicon pickup in molten steel, but also inhibit alumina adhesion inside nozzles, minimizing large-sized inclusions in steel slabs.
Magnesia-carbon submerged entry nozzles avoid alumina contamination in molten steel, effectively improving the quality of tire cord steel.

Production Safety

As materials in direct contact with molten steel, abnormal damage or excessive corrosion of refractories may trigger molten steel leakage and severe safety accidents. Typical hazards include steel breakout caused by over-corroded purging plugs, molten steel splashing from unexpected SEN fracture during service, flow control failure due to severe stopper rod erosion, and steel breakout resulting from side plate malfunction.

Production Efficiency

Refractories for metallurgical furnaces are core consumables in steelmaking, whose performance directly affects production efficiency. Damaged or failed purging plugs and sliding gates require frequent ladle offline replacement and cut down ladle turnover frequency. Submerged entry nozzles, stopper rods and side plates dominate the casting sequence number per tundish. Excessive erosion, molten steel scouring and unexpected fracture of these refractories reduce casting heats and lower overall steel production efficiency.


Tags

Recently Viewed:

  • 菜单

service hotline+86-417-5378688 5378988

Email: guanchengnh@163.com

Address: Boluopu Town, Dashiqiao City, Liaoning Province, China


Copyright © Dashiqiao Guancheng Refractory Co., Ltd. All rights reserved record number:辽ICP备10008524号-4
Disclaimers